Production method of rare earth oxysulfide, ceramic scintillator and its production method, scinti

2025-06-18 10:304010下载
文件类型:PDF文档
文件大小:2465K
A production method of rare earth oxysulfide comprising a step of mixing a rare earth compound with sulfuric acid and/or sulfate in such a proportion that sulfate ions are 0.75-1.75 mol to 1 mol of a rare earth element, thereby preparing a reaction solution to obtain a product; a step of calcining the product to obtain calcined powder; and a step of reducing the calcined powder to obtain rare earth oxysulfide.