文件类型:PDF文档
文件大小:265K
本发明公开了一种抗蠕变耐腐蚀铝合金导体,包括下述重量百分比的组分:Si,0.03‑0.15%;Cu,0.01‑0.25%;Zr,0.02‑0.45%;Fe,0.3‑0.9%;Mg,0.001‑0.012%;B,0.001‑0.015%;稀土元素,0.03‑0.20%;余量为铝和不可避免的杂质。本发明的铝合金导体材料的导电率可达61.9%IACS,抗拉强度可达126MPa,断裂伸长率可达15.6%;具有优异的电导率、柔软性、防腐性和抗蠕变性。