PROBLEM TO BE SOLVED : To provide a method for improving coercive force of magnets.
SOLUTION : The method comprises : a coating step S2) of coating a coating material on a surface of a magnet and drying it; and an infiltrating step S3) of heat treating the magnet obtained from the coating step S2). The coating material comprises (1) metal calcium particles and (2) particles of a material containing a rare earth element. The rare earth element is at least one selected from praseodymium, neodymium, gadolinium, terbium, dysprosium, holmium, erbium, thulium, ytterbium, and lutetium. The method of the present invention can significantly increase coercive force of a permanent magnet material, while remanence and magnetic energy product hardly decrease. In addition, the method of the present invention can significantly decrease the amount of a rare earth element, and accordingly, decrease the production cost.