分享好友 知识库首页 频道列表

Using phosphate, the preparation method, and as this luminophore group of at least one rare earth

2025-06-18 15:254010下载
文件类型:PDF文档
文件大小:259K
Phosphate particulates of at least one rare-earth metal (Ln), with Ln being at least one rare-earth metal selected from among cerium and terbium and optionally lanthanum are in the form of a suspension in a liquid phase of primary isotropic monocrystalline monazite particles having an average size of at least 25 nm and agglomerated into secondary particles having an average size of at most 400 nm; useful luminophores are produced from such phosphate particulates.