A method for flexibly sintering rare earth permanent magnetic alloy comprises : (1) weighing fine powder of rare earth permanent magnetic alloy, loading the fine powder in moulds, and orientedly compacting the fine powder in a press machine and in inert atmosphere to obtain blanks and loading the blanks into charging boxes; (2) opening the two isolating valves connected with each other; wherein after a first rolling wheel transmission in the second conveying vehicle transfers the charging tray into the first chamber of the glove box, the two isolating valves are closed, and the second conveying vehicle leaves; (3) locking two matching flanges of the two isolating valves tightly; (4) locking matching flanges tightly; and (5) processing the blanks with heating and heat preservation according to a preset process curve; wherein the blanks are sintered at a highest temperature of 1200° C.