文件大小:1230K
The present invention provides a semiconductor ceramic composition which is represented by a composition formula of [(Bi-A)x(Ba1-yRy)1-x](Ti1-zMz)aO3 (in which A is at least one kind of Na, Li and K, R is at least one kind of rare earth elements (including Y), and M is at least one kind of Nb, Ta and Sb), in which a, x, y and z satisfy 0.90≤a≤1.10, 0