A method for producing a cold-rolled flat steel product coated with a metallic anticorrosion layer includes producing a steel melt containing in addition to iron and unavoidable impurities (in % by wt.) : C : 0.01-0.35%, Mn : 1-4%, Si : 0.5-2.5%, Nb : to 0.1%, Ti : 0.015-0.1%, P : up to 0.1%, Al : to 0.15%, S : up to 0.01%, N : up to 0.1%, and optionally one or more elements from a group of rare earth metals. The method further includes casting the steel melt to give a preliminary product, hot-rolling the preliminary product to give a hot strip, coiling the hot strip to give a coil, annealing the hot strip, cold-rolling the annealed hot strip to give a cold-rolled flat steel product, finally annealing the cold-rolled flat steel product, and applying a metal anticorrosion layer based on zinc by electrolytic galvanization or hot dip galvanization of the cold-rolled and finally annealed flat steel product.