文件类型:PDF文档
文件大小:435K
PURPOSE : A Sialon phosphor is provided to have a short wavelength of 525-537 nm, and to prevent degradation of color reproducibility and color index.
CONSTITUTION : A Sialon phosphor comprises a compound in chemical formula 1 : Sr_ySi_(6-z)Al_zO_zN_(8-z) : Re_x. In chemical formula 1, x, y and z is respectively 0.005 <= x <= 0.05, 0.05 <= y <= 0.5, 0.001 <= z <= 0.50, and Re is a rare earth element. The rare earth element is selected from a group consisting of Eu and Ce. A manufacturing method of the phosphor comprises : a step of generating a mixture by mixing strontium precursor, silicon precursor, aluminum precursor and precursor of active material, and a step of sintering the mixture under nitrogen atmosphere.
COPYRIGHT KIPO 2012