Method for the preparation of a (green compact) of a magnetic rare earth metal-alloy powder [...], the is comprising the steps of : providing a controlled environment having a temperature of 5 °C -30 °C and a given relative humidity and pressing the rare earth metal-alloy powder within the controlled environment, characterized by, that the relative humidity 40% - 65%.