An electrostatic chuck is provided in which a lower oxide coating, an electrode, and an upper oxide coating are formed on a substrate. The lower oxide coating is formed by spraying an oxide of Gd, Tb, Dy, Ho, Er, Tm, Yb or Lu and has a dielectric strength of 15-50 kV/mm.