A glass having excellent resistance against surface damages is provided. The glass includes a content of alkaline earth oxides of at least 0.3% by weight and of P2O5 of 0.1 to 4% by weight; the glass has at least one surface that has precipitations with a mean size of 1 to 20 μm. A method is further provided and includes melting a glass batch, yielding a glass melt, and casting the glass melt onto a float bath. The glass melt is maintained on the float bath at a temperature of above 1000° C. for at least 5 minutes, and yields glass. The glass has a content of alkaline earth oxides of at least 0.3% by weight and of P2O5 of 0.1 to 4% by weight, and the glass has at least one surface that has precipitations with a mean size of 1 to 20 μm.