Method for manufacturing sintered rare earth magnet

2025-06-19 04:331280下载
文件类型:PDF文档
文件大小:132K
PROBLEM TO BE SOLVED : To manufacture a rare earth sintered magnet using particle having excellent fluidity and is capable of improving size accuracy of a molding body and productivity thereof. SOLUTION : The manufacturing method of rare earth sintered magnet comprises the steps of inputting particles formed of a primary alloy particles of the predetermined composition and an organic solution, obtaining a molding body by impressing a magnetic field to the particles for pressure molding, and sintering the molding body. Here, it is desirable that the organic solution is added in the 1.5 to 15.0 wt% to the primary alloy particle. Moreover, the organic solution of the invention desirably has the characteristics that saturated vapor pressure at 20°C is 75 mmHg (10.0 kPa) or less, surface tension at 20°C is 20 dyn/cm or more and viscosity at 20°C is 0.35 cp or more. COPYRIGHT : (C)2006, JPO&NCIPI