The method for manufacturing an R-Fe-B rare earth magnet of the present invention includes the steps of : compacting rare earth alloy powder having an oxygen content of 4000 wt. ppm or less by dry compacting under compression to produce a compact; impregnating the compact with an oil agent from the surface of the compact; and sintering the compact.