SEMI-CONTINUOUS DUAL-COMPONENT METHOD FOR OBTAINING A POLYURETHANE-MATRIX COMPOSITE EXPLOSIVE CHARGE

2025-06-19 07:131380下载
文件类型:PDF文档
文件大小:1423K
Semi continuous process of forming a composite explosive charge having a charged solid polyurethane matrix comprises : forming a pastry explosive composition (containing a polyol prepolymer, a polyisocyanate monomer, a plasticizer and a pulverulent solid charge having at least one nitro-organic explosive) by continously mixing a liquid component A having the monomer and a pastry component B1 having the prepolymer and the filler in which the plasticizer is distributed between the components; and introducing and thermal crosslinking the composition in to a mould. Semi continuous process of forming a composite explosive charge having a charged solid polyurethane matrix comprises obtaining a pastry explosive composition (containing a polyol prepolymer, a polyisocyanate monomer, a plasticizer and a pulverulent solid charge having at least one nitro-organic explosive) by continously mixing a liquid component A having the monomer at 90-99 wt.% and a pastry component B1 having the prepolymer and the filler together at 1-10 wt.% in which the plasticizer is distributed between the components; introducing the composition in to a mould; and thermal crosslinking the composition in the mould, where the A : B1 weight ratio is 95.05 : 4.95-99.55 : 0.45.


请登录查看


反对 0
举报 0
收藏 0
打赏 0
评论 0