文件类型:PDF文档
文件大小:77K
An acid-resistant glass article is provided comprising : about 25-45 wt-% SiO2; about 20-35 wt-% TiO2; less than about 5 wt-% B2O3; about 15-40 wt-% of an alkaline earth modifier selected from the group consisting of BaO, SrO, and mixtures thereof; and no greater than about 25 wt-% of an alkali-metal oxide selected from the group consisting of Na2O, K2O, and mixtures thereof. The glass article is preferably in the form of a microsphere that is adapted for use as a retroreflective element in pavement markings.