A silicon nitride wear resistant member is composed of a ceramic sintered body containing 55 to 75 mass % of silicon nitride, 12 to 28 mass % of silicon carbide, 3 to 15 mass % of at least one element selected from the group consisting of Mo, W, Ta, and Nb in terms of silicide thereof, and 5 to 15 mass % of grain boundary phase composed of a rare earth element-Si—Al—O—N, the wear resistant member having an electrical resistance of 107 to 104 Ω·cm, a porosity of 1% or less, and a three point bending strength of 900 MPa or more. The wear resistant member has a predetermined electric resistance (electro-conductivity) in addition to the high strength and toughness inherent in silicon nitride per se, especially has a high sliding characteristic. Also, a method of manufacturing the wear resistant member is provided.