PURPOSE : A lead-free brass alloy for globulization of bismuth inclusions is provided that is not harmful to the human body and shows excellent machinability by adding small quantities of bismuth(Bi), misch metal, phosphorous(P) and sulfur(S) except lead(Pb) to a brass alloy consisting of copper(Cu) and zinc(Zn).
CONSTITUTION : A lead-free brass alloy for globulization of bismuth inclusions comprises 50 to 70 wt.% of copper(Cu), 0.5 to 3.5 wt.% of bismuth(Bi), 0.01 to 0.3 wt.% of misch metal, 0.01 to 0.3 wt.% of phosphorous(P) and the balance being zinc(Zn), wherein the lead-free brass alloy further comprises 0.1 wt.% or less of sulfur(S), and wherein the lead-free brass alloy further comprises 1.0 wt.% or less of the sum of iron(Fe) and tin(Sn).