Anode for a high temperature fuel cell and production of same 发明授权

2022-12-22 4650 638K 0

专利信息

申请日期 2025-06-24 申请号 EP10792813
公开(公告)号 EP2502297B1 公开(公告)日 2018-06-06
公开国别 EP 申请人省市代码 全国
申请人 Forschungszentrum Jülich GmbH; Plansee SE
简介 The substrate-supported anode for a high-temperature fuel cell, comprises 3-layer anode laminate (AI, A2, A3) on a metal substrate (S), where the individual layers of the anode laminate each comprise yttrium-oxide-stabilized zirconium dioxide (YSZ) and nickel, a metallic substrate made of chromium based alloy with a chromium content of more than 65 wt.% or a ferritic FeCrMx alloy with a chromium content of 20-30 wt.% and with Mx = an element or an oxide of the group of rare earth metal such as scandium, titanium, aluminum, manganese, molybdenum or cobalt, and a diffusion barrier (D). The substrate-supported anode for a high-temperature fuel cell, comprises 3-layer anode laminate (AI, A2, A3) on a metal substrate (S), where the individual layers of the anode laminate each comprise yttrium-oxide-stabilized zirconium dioxide (YSZ) and nickel, a metallic substrate made of chromium based alloy with a chromium content of more than 65 wt.% or a ferritic FeCrMx alloy with a chromium content of 20-30 wt.% and with Mx = an element or an oxide of the group of rare earth metal such as scandium, titanium, aluminum, manganese, molybdenum or cobalt, and a diffusion barrier (D) arranged between the metallic substrate and the first layer of the anode laminate. The average grain size of the nickel decreases from layer to layer with increasing distance from the substrate. The last layer of the anode laminate, which is intended for contact with the electrolyte has a rootmean- square roughness Rq of less than 4 mu m. The metallic substrate has an average grain size of 20-50 mu m. The last layer of the anode laminate has an average grain size of less than 4 mu m in the nickel phase or an overall average grain size of less than 1.5 mu m. The first layer of the anode laminate has an average grain size of 4-15 mu m in the nickel phase or overall average grain size of 1-8 mu m. The second layer of the anode laminate has an average grain size of 2-7 mu m in the nickel phase or overall average grain size of 0.5-4 mu m. An independent claim is included for a method for producing a substrate-supported anode for a high-temperature fuel cell.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4