NANOCRYSTAL-SIZED CERIUM-ZIRCONIUM-ALUMINUM OXIDE MATERIAL AND METHOD OF MAKING THE SAME 发明申请

2023-03-28 1600 996K 0

专利信息

申请日期 2025-06-26 申请号 US17422770
公开(公告)号 US20220064017A1 公开(公告)日 2022-03-03
公开国别 US 申请人省市代码 全国
申请人 Pacific Industrial Development Corporation
简介 A nanocrystal-sized cerium-zirconium-aluminum mixed oxide material includes at least 20% by mass zirconium oxide; between 5% to 55% by mass cerium oxide; between 5% to 60% by mass aluminum oxide; and a total of 25% or less by mass of at least one oxide of a rare earth metal selected from the group of lanthanum, neodymium, praseodymium, or yttrium. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide exhibits hierarchically ordered aggregates having a dso particle size less than 1.5 μm, and retains at least 80% of surface area and pore volume after ageing at temperature higher than 1000° C. for at least 6 hours. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material is prepared using a co-precipitation method followed by milling the dried and calcined oxide material. The nanocrystal-sized cerium-zirconium-aluminum mixed oxide material forms a particulate filter that may be used in an exhaust system arising from a gas or diesel engine


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4