ANISOTROPIC RARE EARCH MAGNET POWDER, METHOD FOR PRODUCING THE SAME, AND BONDED MAGNET 发明申请

2023-06-05 2500 831K 0

专利信息

申请日期 2025-07-19 申请号 US15484962
公开(公告)号 US20170221618A1 公开(公告)日 2017-08-03
公开国别 US 申请人省市代码 全国
申请人 AICHI STEEL CORPORATION
简介 Anisotropic rare earth magnet powder particles include R2TM14B1-type crystals of a tetragonal compound consisting of one or more rare earth element, B, and one or more transition element, and enveloping layers containing at least Nd and Cu. Surfaces of the R2TM14B1-type crystals are enveloped by the enveloping layers. The particles has an average crystal grain diameter of 0.05 to 1 μm. The particles contain, when the whole particles are taken as 100 atomic %, 11.5 to 15 atomic % of total rare earth element (Rt); 5.5 to 8 atomic % of B; and about 0.05 atomic % to about 2 atomic % of Cu. The powder particles have an atomic ratio of Cu, which is a ratio of the total number of Cu atoms to a total number of atoms of Rt, falling within the range of 1 to 6%. The powder particles do not include dysprosium Dy, Tb, Ho and Ga. Coercivity of the magnetic powder is more than 955 kA/m.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4