Complex oxides for thermal barrier coating having reduced rare-earth contents and pyrochlore-fluorit 发明申请

2023-05-08 1040 557K 0

专利信息

申请日期 2025-08-25 申请号 KR1020160099932
公开(公告)号 KR1020170032836A 公开(公告)日 2017-03-23
公开国别 KR 申请人省市代码 全国
申请人 KOREA INSTITUTE OF CERAMIC ENGINEERING AND TECHNOLOGY
简介 The present invention relates to complex oxide ceramics which have low thermal conductivities and reduced rare-earth contents for high-temperature thermal barrier coatings, and a method of producing the same, and more specifically, to complex oxide ceramics which have low thermal conductivities and pyrochlore-fluorite dual structures for high-temperature thermal barrier coatings, which comprise a composition represented by A_2-_XZr_2_+XO_7+_0.5X (in the formula, A is two elements selected from a group consisting of La, Gd, Sm and Dy, and 0 (AA) Start(BB) End(S10) Two kinds of rare-earth metal oxide powder and ZrO_2 powder in a molar ratio of (2-x) : (4+2x) (0(S20) Mix the rare-earth metal oxide powder with the ZrO_2 powder(S30) Form molded article by using the mixed powder and sinter the sameCOPYRIGHT KIPO 2017


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4