申请日期 | 2025-07-11 | 申请号 | JP2015107787 |
公开(公告)号 | JP2016222947A | 公开(公告)日 | 2016-12-28 |
公开国别 | JP | 申请人省市代码 | 全国 |
申请人 | HONDA MOTOR CO LTD | ||
简介 | PROBLEM TO BE SOLVED : To provide a heat resistant magnesium alloy achieving both of good mechanical property and heat conductivity at high temperature zone of about 200°C without containing rare earth. SOLUTION : There is provided a heat resistant magnesium alloy containing, by mass%, Ca of less than 9.0%, Al of 0.5% or more and less than 5.7%, Si of 1.3% or less and the balance Mg with inevitable impurities with Al+8Ca≥20.5%. SELECTED DRAWING : Figure 1 COPYRIGHT : (C)2017, JPO&INPIT |