IMPROVED WELDING METHOD 发明申请

2023-10-07 2330 468K 0

专利信息

申请日期 2025-08-02 申请号 JP2016089757
公开(公告)号 JP2016209931A 公开(公告)日 2016-12-15
公开国别 JP 申请人省市代码 全国
申请人 Lincoln Global Inc
简介 PROBLEM TO BE SOLVED : To provide an improved welding method. SOLUTION : The present invention, as disclosed herein, generally relates to an improved method of a welding field using a longer distance contact-workpiece longer than one recommended in relation to a shield gas flow rate reduced effectively at a step of adding at least one porosity reducing agent between 0.25 to 10 parts to an electrode composition containing a fluoride lime-based slag, the at least one porosity reducing agent selecting from (a) or (b) and containing the combinations (a) and (b) : (a) one metal nitride forming agent substituting an Li compound, when Al does not exist in at least one metal nitride forming agent in addition to at least one metal nitride forming agent containing an alloy mixing at least one metal alloy or a specific metal out of metals selected from a group consisting of Ti, Zr, Ca, Ba, and Al; and (b) a group consisting of at least one rare earth metal selected from a group composed of La, Ce, Pr, Nd, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Sc, and Y. SELECTED DRAWING : None COPYRIGHT : (C)2017, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4