METHOD FOR REMOVING PHOSPHORUS AND CALCIUM RICH IN RARE EARTH FROM PHOSPHORITE CONTAINING RARE EARTH 发明申请

2023-10-29 4300 762K 0

专利信息

申请日期 2025-06-25 申请号 WOCN15074212
公开(公告)号 WO2016050036A1 公开(公告)日 2016-04-07
公开国别 WO 申请人省市代码 全国
申请人 BEIJING GENERAL RESEARCH INSTITUTE OF MINING AND METALLURGY
简介 A method for removing phosphorus and calcium rich in rare earth from phosphorite containing rare earth through priority leaching by using mixed solution of phosphoric acid and calcium dihydrogen phosphate, mixing phosphorite containing rare earth and cyclical phosphoric acid solution with a solid-liquid ratio of 1 : 2-10, wherein the cyclical phosphoric acid solution contains 15-55 wt% of P2O5, 2-25g/L of Ca2+ and 5-45wt% of effective P2O5; stirring and reacting the mixture at 20-70℃ for 0.5-4 hours; aging for 1-5 hours; and separating the solid and liquid to obtain residue containing enriched rare earth and leaching solution. The leaching solution is mixed with sulfuric acid, and a suitable amount of gypsum residue is added at the same time, wherein mole number of the added sulfuric acid is 0.7-1 time of calcium mole number in the leaching solution, and the amount of the added gypsum residue is 10-100% of the mass of the phosphorite containing rare earth. Recovered phosphoric acid and gypsum residue are obtained by filtering after reaction. Part of recovered phosphoric acid, washing water of the gypsum residue and suitable amount of supplementary water are mixed and returned for leaching as the cyclical phosphoric acid.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4