ALUMINUM ALLOY AND METHOD OF PREPAIRING THE SAME 发明申请

2023-04-17 2980 1303K 0

专利信息

申请日期 2025-09-15 申请号 WOCN15078408
公开(公告)号 WO2015169232A1 公开(公告)日 2015-11-12
公开国别 WO 申请人省市代码 全国
申请人 BYD COMPANY LIMITED
简介 An aluminum alloy contains 1-4wt% of Mn, 0.1-5wt% of Mg, 0.002-0.5wt% of a rare earth element, 0-2wt% of Co, 0-1.5wt% of Fe, 0-1wt% of Ti, 0-1wt% of Cu, 0-1.6wt% of Zn, 0-0.5wt% of Si, and 82.9-98.898wt% of Al, based on total weight of the aluminum alloy. The rare earth element contains La. Based on the total weight of the rare earth element, the content of La in the rare earth element is from 20wt% to 100wt%. A method of preparing an aluminum alloy, a method of coloring a surface of an aluminum alloy and an aluminum alloy product are also provided.