NEODYMIUM-IRON-BORON PERMANENT MAGNET MATERIAL, RAW MATERIAL COMPOSITION THEREFOR AND PREPARATION M 发明申请

2023-02-13 1310 1935K 0

专利信息

申请日期 2026-04-24 申请号 WOCN21095070
公开(公告)号 WO2021238784A1 公开(公告)日 2021-12-02
公开国别 WO 申请人省市代码 全国
申请人 XIAMEN TUNGSTEN CO LTD; FUJIAN CHANGTING GOLDEN DRAGON RARE EARTH CO LTD
简介 Disclosed are a neodymium-iron-boron permanent magnet material, a raw material composition therefor and a preparation method therefor. The raw material composition for preparing the neodymium-iron-boron permanent magnet material comprises the following components : R : 30.2-31.7 mass%, R being a rare earth element; Nb : <0.25 mas% and not 0; Cu : 0.35-0.5 mass%; Al : 0-0.2 mass%; B : 0.92-0.96 mass%; and Fe : 60- 70 mass%. The sum of the components is 100 mass%, R comprises heavy rare earth metal RH, and RH comprises Dy and/or Tb. The square degree of the neodymium-iron-boron permanent magnet material prepared from the raw material composition is 99% or above; the absolute value of the temperature coefficient of Hcj at 20-150°C is 0.404% to 0.414%; the heat treatment temperature range is 470-510°C; Br ≥ 14 kGs, and the coercive force ≥ 25 kOe.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4