简介 |
PROBLEM TO BE SOLVED : To increase a coercive force while minimizing a decline of remanent flux density, in a rare earth permanent magnet.SOLUTION : In a method for producing a rare earth permanent magnet, heat treatment is performed on a sintered magnetic body in a state where a powder mixture is disposed on a surface of the sintered magnetic body, the sintered magnetic body having the composition RTMB(R represents a rare earth element, Trepresents Fe or Co, M represents Al or the like, B represents boron, and a, b, c and d represent atomic percentages which are 12≤a≤20, 0≤c≤10 and 4.0≤d≤7.0 and b is the balance), and the powder mixture containing an Roxide (Rrepresents a rare earth element)and alloy powder having the composition RM, RMHor RTM(Rrepresents a rare earth element, Mrepresents Al or the like, Trepresents Fe and/or Co, and 15
|