METHOD OF MANUFACTURING RARE EARTH MAGNET 发明申请

2023-06-23 3270 1380K 0

专利信息

申请日期 2025-06-28 申请号 WOIB14002800
公开(公告)号 WO2015092524A1 公开(公告)日 2015-06-25
公开国别 WO 申请人省市代码 全国
申请人 TOYOTA JIDOSHA KABUSHIKI KAISHA
简介 A method includes : manufacturing a sintered compact represented by (R1)x(Rh)yTzBsMt and has a grain boundary phase; manufacturing a rare earth magnet precursor from the sintered compact; and performing a heat treatment on the rare earth magnet precursor at 450°C to 700°C to diffuse and to infiltrate a melt of a modified alloy containing a light rare earth element and either a transition metal element, Al, In, Zn, or Ga into the grain boundary phase. R1 represents a light rare earth element. Rh represents Dy or Tb. T represents a transition metal containing at least one of Fe, Ni, and Co. B represents boron. M represents at Ga, Al, or Cu. x, y, z, s, and t represent mass% of R1, Rh, T, B, and M. Following expressions are established : 27≤x≤44, 0≤y≤10, z=100-x-y-s-t, 0.75≤s≤3.4, 0≤t≤3. An infiltration amount of the modified alloy is 0 mass% to 5 mass%.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4