客服热线:18202992950

ACID AND ALKALI RESISTANT NI-CR-MO-CU ALLOYS WITH CRITICAL CONTENTS OF CHROMIUM AND COPPER 发明申请

2023-10-17 2190 652K 0

专利信息

申请日期 2026-03-31 申请号 KR1020130129245
公开(公告)号 KR1020150044356A 公开(公告)日 2015-04-24
公开国别 KR 申请人省市代码 全国
申请人 HAYNES INTERNATIONAL INC
简介 In the field of a waste disposal, a nickel-chrome-molybdenum-copper alloy which is tolerance to sulphuric acid of 70% at 93° C and sodium hydroxide of 50% at 121° C for neutralizing acid and alkali; the alloy contains chrome of 27 to 33 wt.%, molybdenum of 4.9 to 7.8 wt.%, copper of 3.1 to 6.0 wt.% (in the case of chrome of 30 to 33 wt.%), or copper of 4.7 to 6.0 wt.% (in the case of chrome of 27 to 29.9 wt.%), iron of the most 3.0 wt.%, manganese of 0.3 to 1.0 wt.%, aluminium of 0.1 to 0.5 wt.%, silicon of 0.1 to 0.8 wt.%, carbon of 0.01 to 0.11 wt.%, nitrogen of the most 0.13 wt.%, magnesium of the most 0.05 wt.%, a rare-earth element of the most 0.05 wt.%, and the remainder of nickel and impurities. Titanium or another MC carbide former may be added in order to enhance a heat stability.COPYRIGHT KIPO 2015


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4