NICKEL-CHROME-MOLYBDENUM-COPPER ALLOY HAVING ACID RESISTANCE AND ALKALINE RESISTANCE WITH CRITICAL C 发明申请

2023-03-04 4440 569K 0

专利信息

申请日期 2025-07-12 申请号 JP2013224423
公开(公告)号 JP2015078420A 公开(公告)日 2015-04-23
公开国别 JP 申请人省市代码 全国
申请人 HAYNES INTERNATL INC
简介 PROBLEM TO BE SOLVED : To provide an alloy exhibiting resistance to 70% sulphuric acid at 93°C and resistance to 50% sodium hydroxide at 121°C and capable of being proceeded to wrought. SOLUTION : The alloy contains, by weight percent, chrome of 27 to 33, molybdenum of 4.9 to 7.8, copper : 3.1 to 6.0 wt.% when chrome is 30 to 33 wt.% or copper 4.7 to 6.0 wt.% when chrome is 27 to 29.9 wt.%, iron of maximum 3.0, manganese of 0.3 to 1.0, aluminum of 0.1 to 0.5, silicon of 0.1 to 0.8, carbon of 0.01 to 0.11, nitrogen of maximum 0.13, magnesium of maximum 0.05, rare earth element of maximum 0.05 and the balance nickel with impurities. Titanium or other MC-type carbide forming elements can be added for thermal stability improvement of the alloy. COPYRIGHT : (C)2015, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4