氧氮化物半导体薄膜及其制造方法,及薄膜电晶体 发明申请

2023-02-16 1450 3161K 0

专利信息

申请日期 2025-07-20 申请号 TW103107829
公开(公告)号 TW201501211A 公开(公告)日 2015-01-01
公开国别 TW 申请人省市代码 全国
申请人 住友金属鑛山股份有限公司
简介 藉由氧氮化物结晶薄膜,提供一种氧化物半导体薄膜,其具有比较高的载体移动度,适合作为TFT之通道层材料。将含有In、O及N的非晶质之氧氮化物半导体薄膜,或含有In、O、N及添加元素M(M是选自Zn、Ga、Ti、Si、Ge、Sn、W、Mg、Al、Y及稀土类元素的一种以上之元素)之非晶质氧氮化物半导体薄膜,藉由加热温度200℃以上、加热时间1分钟至120分钟的退火处理,获得结晶质之氧氮化物半导体薄膜。 (Problem) ; Providing a suitable oxide semiconductor thin film made of an oxynitride crystalline thin film, which has a relatively higher carrier mobility, and is suitable as channel layer material of TFT. ; (Solution) ; An oxynitride crystalline semiconductor thin film is obtained by a oxynitride annealing amorphous semiconductor thin film at a heating temperature of 200℃ or more, with a heating time of 1 to 120 minutes; the oxynitride crystalline semiconductor thin film includes In, O and N, or includes In, O, N and an additional element M (one or more elements selected from Zn, Ga, Ti, Si, Ge, Sn, W, Mg, Al, Y and rare-earth elements).


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4