简介 A molded rare-earth magnet which simultaneously satisfies increased film thickness, high density, and improved magnetic properties (in particular, coercive force, residual magnetic flux density, and tight adhesion) has a rare-earth magnet phase that contains as a main component a nitride which contains Sm and Fe, in which the molded rare-earth magnet has a density of 80% or higher of the theoretical density of a molded magnet constituted of the rare-earth magnet phase, and has a structure in which particles of Zn and/or Mn have been dispersed in the molded magnet.