申请人 Hitachi Metals Ltd5083
简介 A process for producing an R-Fe-B rare-earth sintered magnet containing at least one lightweight rare-earth element (RL) (at least one of Nd and Pr) and at least one heavy rare-earth element (RH) (at least one of Dy and Tb). An R-Fe-B rare-earth sintered magnet is prepared in which when the contents of the rare-earth element(s), oxygen, carbon, and nitrogen are expressed by X (mass%), ZO (mass%), ZC (mass%), and ZN (mass%), respectively, and ZO+ZC+ZN is expressed by Y (mass%), then the contents satisfy the relationships (0.114X-3.17)=Y=(0.157X-4.27), 0O=0.5, 0C=0.1, and 0N=0.1. Subsequently, a layer rich in the heavy rare-earth element (RH) is formed on the surface of the R-Fe-B rare-earth sintered magnet. The coated R-Fe-B rare-earth sintered magnet is heat-treated at a temperature of 700 to 1, 100°C while holding the magnet with a holding member.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4