For very low hydrogen welding flux-cored wire and its manufacturing method 发明授权

2023-10-27 4710 466K 0

专利信息

申请日期 2025-06-27 申请号 JP2009049398
公开(公告)号 JP5310108B2 公开(公告)日 2013-10-09
公开国别 JP 申请人省市代码 全国
申请人 Sumitomo Metals Co Ltd Nippon Steel6655
简介 PROBLEM TO BE SOLVED : To provide a flux-cored wire for extra-low hydrogen welding, which achieves the welding of high tensile strength steel having tensile strength in a class of ≥690 MPa under a satisfactory welding operation, and to provide a method for producing the same. SOLUTION : Disclosed is a flux-cored wire for extra-low hydrogen welding obtained by filling flux into an outer skin made of steel, which has a composition comprising, by mass% to the total mass of the wire, 0.04 to 0.20% C, 0.1 to 1.5% Si and 0.6 to 2.5% Mn, comprising one or more kinds selected from Mg, Ca, Al, Zr and rare earth metals by 0.01 to 2.00% in total, and the balance iron with inevitable impurities, and in which the value of PTS=C+Si/24+Mn/6+Cu/15+Ni/15+Cr/5+Mo/5+V/5(%) is 0.36 to 1.0 mass% to the whole wire, the total hydrogen content in the wire is ≤6.0 ppm by the mass ratio of the whole wire, and the outer skin made of steel has no slit-shaped joints having the risk of air infiltration. COPYRIGHT : (C)2010, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4