METHOD FOR PRODUCING HIGH-CLEANNESS STEEL 发明申请

2023-10-25 2910 332K 0

专利信息

申请日期 2025-06-28 申请号 KR1020120044605
公开(公告)号 KR1020130087345A 公开(公告)日 2013-08-06
公开国别 KR 申请人省市代码 全国
申请人 JFE STEEL CORPORATION
简介 PURPOSE : A method for producing high-cleanliness steel is provided to reduce manufacturing costs and to produce steel products without defects by increasing the cleanliness of the steel with a circulation-type vacuum degassing device.CONSTITUTION : A method for producing high-cleanliness steel is as follows. In killed treatment, cold materials are added while circulating gas having 4 L(Normal)/min·t or more of flow rate circulates molten steel. While the temperature of the molten steel is adjusted, a circulating time (T) after the addition of the cold materials is set. The circulating time after the addition of the cold materials satisfies next equation. Equation : T (min) >= 0.25 W (kg/t) + 2 In the equation, W means an amount of the added cold materials per 1 ton of the molten steel.[Reference numerals] (AA) Backflow gas flow rate : 8L(Normal)/min·t; (BB) Backflow time after inserting a refrigerant(min); (CC) Rate of inclusion generation 0.01 piece /cm^2; (EE) Refrigerant input amountCOPYRIGHT KIPO 2013


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4