客服热线:18202992950

ANISOTROPIC RARE EARTH BOND MAGNET AND METHOD FOR MANUFACTURING THE SAME 发明申请

2023-03-19 3250 106K 0

专利信息

申请日期 2025-07-14 申请号 JP2010175039
公开(公告)号 JP2013145769A 公开(公告)日 2013-07-25
公开国别 JP 申请人省市代码 全国
申请人 KRI INC
简介 PROBLEM TO BE SOLVED : To provide an anisotropic bond magnet provided with high magnetic characteristics, temperature characteristics and corrosion resistance by recycling municipal scraps of rare earth sintered magnets at low cost. SOLUTION : A method for manufacturing an anisotropic rare earth bond magnet includes the steps of : mechanically pulverizing rare earth magnets in an inert atmosphere; performing annealing treatment for eliminating strains to the pulverized material at a temperature from 400°C to 600°C during a retention time of 12 hours or more in a high vacuum or inert atmosphere; and kneading a binder and the material having been subjected to the annealing treatment for eliminating strains to be subjected to magnetic field molding. The method eliminates separation/purification of Sm and Nd, peeling of a magnet surface processing coating such as Ni plating, and removal of an adhesive. COPYRIGHT : (C)2013, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4