客服热线:18202992950

Flux-cored wire for stainless steel arc welding 发明授权

2023-09-30 1620 677K 0

专利信息

申请日期 2025-06-24 申请号 US12955393
公开(公告)号 US8492679B2 公开(公告)日 2013-07-23
公开国别 US 申请人省市代码 全国
申请人 Hiroshi Sugahara; Tetsunao Ikeda; Hirohisa Watanabe
简介 A flux-cored wire for stainless steel arc welding including an outer sheath made of stainless steel and flux filled up in the outer sheath contains, as percentage to the total mass of the wire, Cr : 22.0-30.0 mass %, Ni : 6.0-12.0 mass %, Mo : 2.0-5.0 mass %, N : 0.20-0.35 mass %, TiO2 : 4.0-9.0 mass %, SiO2 : 0.1-2.0 mass %, ZrO2 : 0.5-4.0 mass %, total of Li2O, Na2O and K2O : 0.50-1.50 mass %, metal fluoride in terms of fluorine amount : 0.10-0.90 mass %, and rare earth element component : 0.10-1.00 mass %, limits C to 0.04 mass % or below, W to 4.0 mass % or below, Cu to 2.0 mass % or below, Bi2O3 to 0.01 mass % or below, and limits oxides other than the above to 3.0 mass % or below. With such a composition, it is possible to obtain a weld bead which is excellent in the weldability in welding in all attitudes and is more excellent in the low temperature toughness while keeping excellent pitting corrosion resistance in arc welding of duplex stainless steel and the like.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4