客服热线:18202992950

The method for producing the same hydraulic pressure and high tensile steel and iron 发明授权

2023-03-23 2040 198K 0

专利信息

申请日期 2025-07-01 申请号 JP2009054418
公开(公告)号 JP5206507B2 公开(公告)日 2013-06-12
公开国别 JP 申请人省市代码 全国
申请人 Sumitomo Metals Co Ltd Nippon Steel6655
简介 PROBLEM TO BE SOLVED : To provide a high tensile strength steel material for a hydraulic pressure iron pipe having excellent weld zone toughness, further free from the generation of weld cracking even if welding is performed in a preheating-free state under a high temperature-high humidity environment, and is further friendly to natural environment. ŽSOLUTION : The high tensile strength steel material for the hydraulic pressure iron pipe has a chemical composition containing 0.04 to 0.09% C, 0.05 to 0.6% Si, 1.0 to 1.8% Mn, ≤0.02% P, ≤0.01% S, COPYRIGHT : (C)2010, JPO&INPIT Ž