The rare earth element and an alloy of nickel-titanium-alloy treatment method 发明申请

2023-05-26 1220 1506K 0

专利信息

申请日期 2025-07-07 申请号 JP2012539961
公开(公告)号 JP2013510955A 公开(公告)日 2013-03-28
公开国别 JP 申请人省市代码 全国
申请人 COOK MEDICAL TECHNOLOGIES LLC
简介 A nickel-titanium-rare earth (Ni-Ti-RE) alloy comprises nickel at a concentration of from about 35 at. % to about 65 at. %, a rare earth element at a concentration of from about 1.5 at. % to about 15 at. %, boron at a concentration of up to about 0.1 at. %, with the balance of the alloy being titanium. In addition to enhanced radiopacity compared to binary Ni-Ti alloys and improved workability, the Ni-Ti-RE alloy preferably exhibits superelastic behavior. A method of processing a Ni-Ti-RE alloy includes providing a nickel-titanium-rare earth alloy comprising nickel at a concentration of from about 35 at. % to about 65 at. %, a rare earth element at a concentration of from about 1.5 at. % to about 15 at. %, the balance being titanium; heating the alloy in a homogenization temperature range below a critical temperature; and forming spheroids of a rare earth-rich second phase in the alloy while in the homogenization temperature range.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4