Dielectric ceramic and laminated ceramic capacitor using the same 发明授权

2023-03-30 1690 97K 0

专利信息

申请日期 2025-07-07 申请号 JP2008167420
公开(公告)号 JP5164687B2 公开(公告)日 2013-03-21
公开国别 JP 申请人省市代码 全国
申请人 Kyocera6633
简介 Disclosed is a dielectric ceramic having crystal grains mainly composed of barium titanate and an intergranular phase present among the crystal grains. The dielectric ceramic contains, per 100 moles of barium constituting the barium titanate, 0.05-0.3 mole of vanadium in terms of V2O5, and 0.5-1.5 moles of one rare earth element (RE) selected from yttrium, dysprosium, holmium and erbium in terms of RE2O3. In an x-ray diffraction chart, the diffraction intensity of the (004) plane indicating tetragonal barium titanate is higher than the diffraction intensity of the (400) plane indicating cubic barium titanate. The dielectric ceramic has a Curie temperature of 100-120°C.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4