简介 In a nanocomposite bulk magnet according to the present invention, nanocomposite magnet powder particles, including an Nd2Fe14B crystalline phase and an α-Fe phase, are combined together. The composition of the magnet is represented by T100-x-y-z-n(B1-qCq)xRyTizMn, where T is at least one transition metal element selected from the group consisting of Fe, Co and Ni and always including Fe, R is at least one rare-earth element including substantially no La or Ce, M is an additive metallic element, and x, y, z, n and q satisfy 4 at %≰x≰10 at %, 6 at %≰y≰10 at %, 0.05 at %≰z≰5 at %, 0 at %≰n≰10 at %, and 0≰q≰0.5, respectively. The powder particles have a minor-axis size of less than 40 μm. And powder particles, of which the major-axis size exceeds 53 μm, account for at least 90 mass % of the entire magnet. And those powder particles are directly combined with each other. Consequently, a full-dense magnet, of which the density is 96% or more of the true density of its material alloy, is realized.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4