RARE-EARTH SINTERED MAGNET, METHOD OF MANUFACTURING THE SAME, AND ROTARY MACHINE 发明申请

2023-01-29 1720 189K 0

专利信息

申请日期 2025-06-26 申请号 JP2010075413
公开(公告)号 JP2011210838A 公开(公告)日 2011-10-20
公开国别 JP 申请人省市代码 全国
申请人 TDK CORP
简介 PROBLEM TO BE SOLVED : To provide a rare-earth sintered magnet capable of obtaining superior HcJ, while maintaining high Br. SOLUTION : A rare-earth sintered magnet having a composition containing a rare-earth element, a transition element and boron, includes a heavy rare-earth element and a light rare-earth element as rare-earth elements. The rare-earth sintered magnet is configured by a crystal grain having a composition containing the rare-earth element, the transition element, and boron and a grain boundary region formed between the crystal grains. A triple point region, that is a grain boundary region surrounded by three or more crystal grains, contains the rare-earth element, the transition element, and boron, and has a composition different from that of the crystal grain. The average area of the triple point region is 3.0 μm2 or less, when it is measured in an arbitrary surface or in a cross section, and the standard deviation of distribution of the area is 5 or less. COPYRIGHT : (C)2012, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4