简介 A nanocomposite magnet according to the present invention has a composition represented by the general formula : RxQyMz(Fe1-mTm)bal, where R is at least one rare-earth element, Q is at least one element selected from the group consisting of B and C, M is at least one metal element that is selected from the group consisting of Al, Si, Ti, V, Cr, Mn, Cu, Zn, Ga, Zr, Nb, Mo, Ag, Hf, Ta, W, Pt, Au and Pb and that always includes Ti, and T is at least one element selected from the group consisting of Co and Ni. The mole fractions x, y, z and m satisfy the inequalities of 6 at %≰x<10 at %, 10 at %≰y≰17 at %, 0.5 at %≰z≰6 at % and 0≰m≰0.5, respectively. The nanocomposite magnet includes a hard magnetic phase and a soft magnetic phase that are magnetically coupled together. The hard magnetic phase is made of an R2Fe14B-type compound, and the soft magnetic phase includes an α-Fe phase and a crystalline phase with a Curie temperature of 610° C. to 700° C. (ω phase) as its main phases.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4