Method and device for manufacturing a sintered rare earth magnet 发明授权

2023-12-22 2510 98K 0

专利信息

申请日期 2025-06-24 申请号 JP2004096378
公开(公告)号 JP4591748B2 公开(公告)日 2010-12-01
公开国别 JP 申请人省市代码 全国
申请人 TDK Corporation3067
简介 PROBLEM TO BE SOLVED : To prevent the generation of cracks in sintering and to improve material yield. ŽSOLUTION : In the method, a molded item formed by molding a raw material including a rare earth element is sintered and a rare earth sintered magnet is obtained. The molded item is ground and processed in non-oxide atmosphere before sintering and cut powder generated by grinding is collected and reused. In the non-oxide atmosphere in grinding, the oxygen concentration is 50 to 30, 000 ppm. The maximum compression ratio of the molded item is at most 5. The profile of a cutting tool used for grinding is 0.01 to 0.05 mm. The peripheral speed of the cutting tool used for grinding is 200 to 1, 700 m/minute. The feed speed of the molded item is 300 to 4, 200 mm/minute. ŽCOPYRIGHT : (C)2006, JPO&NCIPI Ž


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4