申请人 SUMITOMO METAL IND
简介 PROBLEM TO BE SOLVED : To provide a high tensile strength steel material for a hydraulic pressure iron pipe having excellent weld zone toughness, further free from the generation of weld cracking even if welding is performed in a preheating-free state under a high temperature-high humidity environment, and is further friendly to natural environment. SOLUTION : The high tensile strength steel material for the hydraulic pressure iron pipe has a chemical composition containing 0.04 to 0.09% C, 0.05 to 0.6% Si, 1.0 to 1.8% Mn, ≤0.02% P, ≤0.01% S, <0.005% Nb, 0.002 to 0.07% Al, 0.001 to 0.005% N, and the balance Fe with impurities, and produced by being subjected to hot working after heating to a temperature of 850 to <1, 000°C. The steel material may have a chemical composition comprising one or more kinds of elements selected from Cu, Ni, Cr, Mo, V, Ti, B, Ca, Mg and rare earth metals. COPYRIGHT : (C)2010, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4