ALLOY, PROTECTIVE LAYER AND COMPONENT 发明申请

2023-10-01 2740 354K 0

专利信息

申请日期 2025-07-07 申请号 WOEP10050266
公开(公告)号 WO2010086212A1 公开(公告)日 2010-08-05
公开国别 WO 申请人省市代码 全国
申请人 SIEMENS AG; STAMM WERNER
简介 Known protective layers with a high Cr content and additionally silicon form brittle phases that become more brittle under the influence of carbon during use. The protective layer according to the invention has the composition 24% to 26% cobalt (Co), 9% to 12% aluminium (Al), 0.1% to 0.7% yttrium (Y) and/or at least one equivalent metal from the group comprising scandium and rare earth elements, 16% to 25% chromium (Cr), optionally 1.0% to 4.0% rhenium, optionally 0.1% to 0.7% phosphorus, optionally 0.2% to 0.6% silicon, and nickel making up the remainder.