Austenitic stainless steel welded joint and austenitic stainless steel welding material 发明申请

2023-01-31 3120 927K 0

专利信息

申请日期 2025-06-25 申请号 US12458507
公开(公告)号 US20100062279A1 公开(公告)日 2010-03-11
公开国别 US 申请人省市代码 全国
申请人 OSUKI TAKAHIRO; OGAWA KAZUHIRO; OKADA HIROKAZU; IGARASHI MASAAKI
简介 An austenitic stainless steel welded joint, whose base metal and weld metal each comprises, by mass percent, C : not more than 0.3%, Si : not more than 2%, Mn : 0.01 to 3.0%, P : more than 0.04% to not more than 0.3%, S : not more than 0.03%, Cr : 12 to 30%, Ni : 6 to 55%, rare earth metal(s) : more than 0.2% to not more than 0.6%, sol. Al : 0.001 to 3% and N : not more than 0.3%, with the balance being Fe and impurities, and satisfies the formula of (Cr+1.5×Si+2×P)/(Ni+0.31×Mn+22×C+14.2×N+5×P)<1.388, in spite of having a high P content and showing the fully austenitic solidification, has excellent resistance to the weld solidification cracking. Therefore, the said austenitic stainless steel welded joint can be widely used in such fields where a welding fabrication is required. Each element symbol in the above formula represents the content by mass percent of the element concerned.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4