Method and device for manufacturing sintered rare earth magnet of the magnetic anisotropy 发明授权

2023-08-13 2250 476K 0

专利信息

申请日期 2025-09-08 申请号 JP2005322921
公开(公告)号 JP4391980B2 公开(公告)日 2009-12-24
公开国别 JP 申请人省市代码 全国
申请人 INTER METALLICS KK
简介 PROBLEM TO BE SOLVED : To provide a method of manufacturing a magnetically anisotropic rare earth sintered magnet and an efficient method of manufacturing products of various shapes that are effective for improving the performance of rare earth magnets, and can safely use extremely active powder in which the degree of oxidation is low and the particle diameter is extremely small. SOLUTION : In the manufacturing method, fine powders available as materials for magnetically anisotropic rare earth sintered magnets are filled into a mold up to a predetermined density in a weighing/filling section 41 and a densification section 42, fine powders are oriented by a pulse magnetic field at a magnetic field orientation section 43, and then the fine powders are sintered in a sintering furnace 44 without pressing. Since the operation of a mass-producing apparatus is simple in this method, an enclosure can be made smaller, thus excluding the risk of oxidation and combustion of the powder, which has been the problem in a conventional method using a large-scale press. A product in the most important shape in a rare earth sintered magnet, such as a flat-plate-shaped/bow-plate-shaped magnet, can be manufactured efficiently by a multi-cavity mold. COPYRIGHT : (C)2007, JPO&INPIT


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4