R-Fe-B magnet working method 发明授权

2023-02-15 2220 35K 0

专利信息

申请日期 2025-07-30 申请号 JP11102307
公开(公告)号 JP4379754B2 公开(公告)日 2009-12-09
公开国别 JP 申请人省市代码 全国
申请人 SUMITOMO SPEC METALS
简介 PROBLEM TO BE SOLVED : To markedly reduce adherence of concentrated ions to prevent roughened plated surface and generation of rust by immersing a machine a workpiece of an R-Fe-B sintered magnet body into a grinding and rust- preventing oil, then barrel-polishing it in a barrel machine in which the grinding and rust-preventing oil is filled, and then cleaning and drying it. SOLUTION : R-Fe-B (R includes Y, and contains at least one or more are earth elements including a light are earth element and a heavy rare earth element) magnet powder having required composition is press-molded into a long bow shape, sintered, and subjected to aging, then the inner surface R, outer surface R, and required thickness of the magnet long size blank are polished in this order with a rust preventing oil, and then the workpiece is immersed into a polishing and rust-preventing oil to remove the grinding scraps or polishing scraps, etc. Then, the workpiece is beveled by barrel-polishing it in a barrel machine in which the grinding and rust-preventing oil is received in a state wherein the workpiece is coated with the grinding and rust-preventing oil. Then, after the magnet is cleaned by being exposed to a jet of or immersed into water into which N2 gas is injected, it is dried and subjected to following plating treatment.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4