Fireable, low melting nickel-chrome alloy for manufacturing ceramic lined dental restorations 发明授权

2023-11-09 4770 381K 0

专利信息

申请日期 2025-07-18 申请号 EP07102905
公开(公告)号 EP1961407B1 公开(公告)日 2009-12-02
公开国别 EP 申请人省市代码 全国
申请人 BEGO Bremer Goldschlägerei Wilh Herbst GmbH Co KG
简介 Fireable alloy (I) to prepare dental restoration blended with ceramic material, comprises +- 37, preferably 18-23.5 wt.% of nickel-chromium; 8-16 wt.% of molybdenum and tungsten; 0.5-3.4, preferably 2.1-3.4 wt.% of silicon and 0.31-2.5 wt.% or 0-0.05 wt.% of boron; 0-0.9 wt.% of niobium; 0-0.5 wt.% of manganese; 0-0.02 wt.% of carbon; 0-30 wt.% of iron, cobalt and copper; 0-0.5 wt.% of aluminum, titanium, zirconium, hafnium, yttrium, lanthanum, cerium, other rare earth metals, calcium and strontium; 0-0.3 wt.% of beryllium; and 0-10 wt.% of other metal, metalloids and other ingredients. An independent claim is included for a ceramic blended dental restoration comprising a scaffold of (I); and a dental ceramic with a heat expansion coefficient of 12-14 [10 6>K ->1] at 25-500[deg] C, which is calcined on the scaffold.


您还没有登录,请登录后查看下载地址


反对 0举报 0 收藏 0 打赏 0评论 0
下载排行
网站首页  |  关于我们  |  联系方式  |  使用协议  |  版权隐私  |  网站地图  |  排名推广  |  广告服务  |  积分换礼  |  网站留言  |  RSS订阅  |  违规举报  |  京ICP备2021025988号-4